2026-11-27 at 12:00 am #14262
Published: November 2026 | By Gold Auto Parts Engineering Team
Two ratios decide whether a thin-wall tube can be bent, and the trade gives both of them the same name. Tube benders say wall factor and mean OD / t — the number that tells you whether the wall can support itself. Piping engineers say wall factor and mean CLR / OD. We receive RFQs written in both conventions every week, and a part quoted off the wrong axis can put 40% of tooling cost in the wrong place.
So this article separates them and then puts them back together on one grid — the wall factor CLR to OD ratio chart we use to answer "can this be bent" before a die is cut. Read it as the map of a process window rather than a rule book: every cell names the tooling set that holds the part, because on thin wall the tooling is what decides the answer.

1. Which Ratio Is "Wall Factor" — and Why Do Two Charts Disagree?
Because they describe two different failures. OD / t governs collapse and wrinkling on the intrados: a wall that is too thin relative to the diameter buckles before the bend reaches 60°. CLR / OD governs how much the section has to distort, and therefore ovality and extrados thinning. A part passes only when both are satisfied, which is why a single-axis chart is always wrong somewhere.
For a 25 × 0.9 mm tube, OD / t is 27.8 and CLR / OD at 1.5D is 1.5. Multiply the two ratios and you get the K index used in piping design — 0.054 here — where anything at or below 0.10 is classed as infeasible. Automotive practice reaches about 0.045, so the index is roughly twice as conservative as a modern ball-mandrel machine. That gap is the whole subject of thin wall bending, and it is why the bend radius to wall thickness ratio steel tube buyers actually ask for sits inside a region the piping chart calls impossible.
Three inputs move a part one cell in either direction, and none of them appears on the drawing:
• Wall eccentricity. A coil at 10% eccentricity behaves like a thinner nominal wall on one side of the circumference. EN 10305-1 allows 10%; we ask for 5% on 0.9 mm work.
• Temper. An as-drawn BK tube carries 1–1.5° more springback than an annealed GBK, and springback comes out of the leg position, not the angle.
• Seam. On welded tube the seam must face the neutral axis. On a 1.0D bend there is no neutral axis left to hide it in, which is why our factory specifies seamless below 1.2D.
✅ Bottom line: OD/t tells you if the wall survives, CLR/OD tells you if the section survives, and the tooling set is what reconciles them.
2. The Table: CLR/OD Against t/D for 25 mm Tube
Each cell names the tooling that holds the part in production, not a verdict. That is the practical difference between this wall factor CLR to OD ratio chart and the ones built from theory: 1.5D bend radius thin wall feasibility is not a property of the radius, it is a property of the radius plus the recipe beside it.
R/D ↓ t/D → 0.020 0.030 0.040 0.050 0.060 0.080 1.0 ✗ B4+ B4+ B4+ B3+ B2 1.2 B4+ B4+ B4+ B3+ B2 P 1.5 B4+ B3+ B3+ B2 B2 P 2.0 B3+ B3+ B2 B2 P P 2.5 B3+ B2 B2 P P P 3.0 B3+ B2 P P P P P plug mandrel. B2 two-ball mandrel and wiper die. B3+ three-ball mandrel, wiper, 40% axial boost. B4+ four-ball mandrel, wiper, 60% boost, bend speed halved. ✗ not a rotary draw part at that geometry — hydroforming or press bending territory.
Read three rows off it. A 25 × 0.9 mm link at 1.5D sits between the 0.030 and 0.040 columns and lands on B3+ — three balls, wiper, 40% boost. The same tube at 1.2D drops to B4+, and at 2.0D it relaxes to B2 or B3+. A 1.2 mm wall at 1.5D sits on the B2 side of that boundary, which is why the 1.2 mm line is cheaper to quote and far less sensitive to tube condition. A 2.0 mm wall is plug territory from 1.5D outward.
Difficulty rises toward the top left, where both ratios work against you, and the single ✗ sits at 1.0D on 0.020 t/D. The K index is just the product of the two axes, so its contours run diagonally — which is why a shop quoting by K alone gets the top-left corner wrong and the rest roughly right.
✅ Bottom line: 0.9 mm on 25 mm holds 1.5D with three balls, a wiper and 40% boost — the radius is not what limits it, the recipe is.
3. How Do I Use a Cell Without Getting Burned?
Four steps, and the first one costs nothing:
• Compute both ratios from the drawing — OD/t and CLR/OD — and find the cell before you ask anyone for a price. A quote that ignores the cell is a quote for a different part.
• Check the tube certificate against the assumptions — eccentricity, temper, seamless or welded. The bend radius to wall thickness ratio steel tube holds on paper is only true for a wall that is concentric and annealed.
• Ask for three numbers, not a capability statement: ovality, extrados thinning and Cpk on bend angle, from a 30-piece run. A supplier who cannot produce them has not run the cell.
• Price the recipe, not just the part. A B4+ cell needs slower cycle time and more tooling than a B2 cell on the same drawing — 30 to 60% more per piece at low volume, narrowing to 10–15% above 20,000 units.
Suzhou Gold Auto Parts Co., Ltd. works from this grid on every OEM and custom enquiry: the cell decides the tooling list, the tooling list decides the piece price, and the buyer sees both lines separately. It is also why two Gold Auto Parts quotes on similar drawings can differ — they sit in different cells.
Frequently Asked Questions
Q: Is wall factor OD/t or CLR/OD?
A: Both are in use, which is exactly why a wall factor CLR to OD ratio chart has to label its axes. In tube bending shops wall factor is OD/t and the radius is quoted as a multiple of diameter. In piping and pressure-vessel work the same words often mean CLR/OD. When an RFQ is ambiguous, quote the two numbers explicitly and the ambiguity disappears.
Q: What is the tightest bend for a 25 × 0.9 mm tube?
A: 1.2D is marginal — B4+, four-ball mandrel, 60% boost, and extrados thinning that lands near the 15% limit. 1.5D is the production floor and the number we would put on a drawing. Below 1.2D, 1.5D bend radius thin wall feasibility stops being the question, because rotary draw stops being the process.
Q: Why does the same cell behave differently at two suppliers?
A: Because the cell assumes a tube, and the tube is the variable nobody puts in the RFQ. Eccentricity, temper and seam position move a part one grade either way, and boost pressure is often set by feel rather than by number. Gold Auto Parts specifies 5% eccentricity and annealed GBK on every 0.9 mm order, which is why our B3+ cell repeats and someone else's does not.
Find Your Cell
Send the tube OD, wall and centreline radius, and Suzhou Gold Auto Parts Co., Ltd. — a China manufacturer bending 0.9 mm and 1.2 mm wall — will tell you which cell you are in, what tooling it needs and where the radius has to move to drop a grade. Within two working days, free.
The formed tube components we bend today sit across this grid; the 0.9 mm thin-wall connecting rod is the B3+ case and the 1.2 mm large-radius rod shows what dropping to B2 buys you. For what the cell costs in money rather than tooling, see our 2026 price ranges by volume.
Send your tube size for a free cell check →